Brand Name : Tankii
Model Number : 1cr20al3 0cr25al5 0Cr21Al6Nb
Place of Origin : China
MOQ : 10kg
Price : 5usd/kg
Payment Terms : L/C, D/P, T/T, Western Union
Supply Ability : 100ton/month
Delivery Time : 5-15days
Packaging Details : Standard
C | P | S | Mn | Si | Cr | Ni | Al | Fe | Other | ||
Max | |||||||||||
0.05 | 0.025 | 0.025 | 0.70 | Max 0.6 | 21.0~23.0 | Max 0.60 | 5.0~7.0 | Bal. | Nb 0.5 |
Max Continuous Service Temp | 1350ºC |
Resisivity at 20ºC | 1.45 ohm mm2/m |
Density | 7.1 g/cm3 |
Thermal Conductivity | 46.1 KJ/m·h·ºC |
Coefficient of Thermal Expansion | 16.0×10-6/ºC |
Melting Point | 1510ºC |
Tensile Strength | 637~784 Mpa |
Elongation | Min 12% |
Section Variation Shrink Rate | 65~75% |
Repeatedly Bend Frequency | Min 5 times |
Continuous Service Time | - |
Hardness | 200-260HB |
Micrographic Structure | Ferrite |
Magnetic Property | Magnetic |
Grade | Highest temperature | Resistivity | Melting point | Tensile strength | Elongation |
0Cr21Al4 | 1100ºC | 1.23±0.06μΩ.m | 1500ºC | 750 | ≥12 |
0Cr25Al5 | 1250ºC | 1.42±0.07μΩ.m | 1500ºC | 750 | ≥12 |
0Cr21Al6NbCo | 1350ºC | 1.43±0.07μΩ.m | 1510ºC | 750 | ≥12 |
0Cr27Al7Mo2 | 1400ºC | 1.53±0.07μΩ.m | 1520ºC | 750 | ≥10 |
KSC | 1350ºC | 1.44±0.05μΩ.m | 1510ºC | 750 | ≥16 |
Cr20Ni80 | 1200ºC | 1.09±0.05μΩ.m | 1400ºC | 750 | ≥20 |
Cr15Ni60 | 1150ºC | 1.12±0.05μΩ.m | 1390ºC | 750 | ≥20 |
Cr20Ni35 | 1100ºC | 1.04±0.05μΩ.m | 1390ºC | 750 | ≥20 |
Cr20Ni30 | 1100ºC | 1.04±0.05μΩ.m | 1390ºC | 750 | ≥20 |
Grade | Chemical composition% | ||||||||
C | P | S | Mn | Si | Cr | Ni | Al | Fe | |
≤ | |||||||||
0Cr21Al4 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.0 | 17-21 | ≤0.6 | 3-4 | balance |
0Cr25Al5 | 0.06 | 0.025 | 0.02 | 0.5 | ≤0.6 | 23-26 | ≤0.6 | 4.5-6.5 | balance |
0Cr21Al6Nb | 0.05 | 0.025 | 0.02 | 0.5 | ≤0.6 | 21-23 | ≤0.6 | 5-7 | balance |
0Cr27Al7Mo2 | 0.05 | 0.025 | 0.02 | 0.2 | ≤0.4 | 26.5-27.8 | ≤0.6 | 6-7 | balance |
Cr20Ni80 | 0.08 | 0.02 | 0.015 | 0.6 | 0.75-1.6 | 20-23 | balance | <0.5 | ≤1.0 |
Cr15Ni60 | 0.08 | 0.02 | 0.015 | 0.6 | 0.75-1.6 | 15-18 | 55-61 | <0.5 | balance |
Cr20Ni35 | 0.08 | 0.02 | 0.015 | 1.0 | 1-3 | 18-21 | 34-37 | - | balance |
Cr20Ni30 | 0.08 | 0.02 | 0.015 | 1.0 | 1-3 | 18-21 | 30-34 | - | balance |